Differential Scanning Calorimetry

Panoramica

Source: Danielle N. Beatty and Taylor D. Sparks, Department of Materials Science and Engineering, The University of Utah, Salt Lake City, UT

Differential scanning calorimetry (DSC) is an important measurement to characterize thermal properties of materials. DSC is used primarily to calculate the amount of heat stored in a material as it heats up (heat capacity) as well as the heat absorbed or released during chemical reactions or phase changes. However, measurement of this heat can also lead to the calculation of other important properties such as glassy transition temperature, polymer crystallinity, and more.

Due to the long, chain-like nature of polymers it is not uncommon for polymer strands to be entangled and disordered. As a result, most polymers are only partially crystalline with the remainder of the polymer being amorphous. In this experiment we will utilize DSC to determine polymer crystallinity.

Procedura
  1. Turn on the machine and allow it to warm up for about an hour.
  2. Check to ensure the compressed nitrogen tank and liquid nitrogen tank are both full and the valve connecting them is open. The compressed nitrogen pressure flow is set at 10 psi by the adjustment knobs on the regulator.
  3. Prepare two empty pans. Poke a small hole in the lid of each and seal by using the crimping press. Remove the three furnace lids and place the pans on the two circular sensors within the furnace. Replace all three lids.
  4. Click o

Log in or to access full content. Learn more about your institution’s access to JoVE content here

Risultati

Figure 3 shows the result of a DSC percent crystallinity sample scan on a polybutylene terephthalate (PBT) polymer sample. The result is displayed as a DSC power reading (in milliwatts per milligram of sample) verses time. The power reading, the blue trace in Figure 3, indicates how much additional power was required to change the temperature of the sample pan in comparison to the empty reference pan. The temperature program is a

Log in or to access full content. Learn more about your institution’s access to JoVE content here

Tags
Differential Scanning CalorimetryDSCThermal PropertiesMaterialsPolymersMeasurement TechniqueSample PanReference PanTemperature SensorsHeatersEnergy FlowPhase ChangeReactionPolymer Phase TransitionsPercent CrystallinityCrystalline PolymersAmorphous PolymersMeltingGlass Transition

Vai a...

0:08

Overview

1:26

Principles of DSC Analysis of Polymers

3:51

DSC Baseline Measurement

6:52

DSC Sample Measurement

8:21

Analysis of the DSC Data

9:33

Applications

11:29

Summary

Video da questa raccolta:

article

Now Playing

Differential Scanning Calorimetry

Materials Engineering

36.9K Visualizzazioni

article

Optical Materialography Part 1: Sample Preparation

Materials Engineering

15.3K Visualizzazioni

article

Optical Materialography Part 2: Image Analysis

Materials Engineering

10.9K Visualizzazioni

article

X-ray Photoelectron Spectroscopy

Materials Engineering

21.5K Visualizzazioni

article

X-ray Diffraction

Materials Engineering

87.9K Visualizzazioni

article

Focused Ion Beams

Materials Engineering

8.8K Visualizzazioni

article

Directional Solidification and Phase Stabilization

Materials Engineering

6.5K Visualizzazioni

article

Thermal Diffusivity and the Laser Flash Method

Materials Engineering

13.1K Visualizzazioni

article

Electroplating of Thin Films

Materials Engineering

19.6K Visualizzazioni

article

Analysis of Thermal Expansion via Dilatometry

Materials Engineering

15.6K Visualizzazioni

article

Electrochemical Impedance Spectroscopy

Materials Engineering

23.0K Visualizzazioni

article

Ceramic-matrix Composite Materials and Their Bending Properties

Materials Engineering

8.0K Visualizzazioni

article

Nanocrystalline Alloys and Nano-grain Size Stability

Materials Engineering

5.1K Visualizzazioni

article

Hydrogel Synthesis

Materials Engineering

23.5K Visualizzazioni

JoVE Logo

Riservatezza

Condizioni di utilizzo

Politiche

Ricerca

Didattica

CHI SIAMO

Copyright © 2025 MyJoVE Corporation. Tutti i diritti riservati