Differential Scanning Calorimetry (DSC) is a method of thermodynamic analysis based on heat-flux method, wherein a sample material (enclosed in a pan) and an empty reference pan are subjected to identical temperature conditions. The energy difference that is required to maintain both the pans at the same temperature, owing to the difference in the heat capacities of the sample and the reference pan, is recorded as a function of temperature. This energy released or absorbed is a measure of the enthalpy change (ΔΗ) of the sample with respect to the reference pan.

Procedimento

1. Baseline Measurement

  1. Controller, Measuring unit, Computer system, Thermostat approximately 60 min. before starting the measurement. Purge gases must be connected to the system.
  2. Place two empty crucibles (with lid) into the sample carrier. The crucible material may be chosen based on the temperature range to be measured.
  3. Move the furnace to measuring position.
  4. Adjust the measuring conditions (gas, vacuum).
  5. Start the measurement program.
  6. Proceed to create a b

Log in or to access full content. Learn more about your institution’s access to JoVE content here

Resultados

ZnO formation via Decomposition of ZnCO3

The change in enthalpy per degree, at constant pressure is equivalent to the heat capacity of a material at constant pressure given by Equation 1. The enthalpy change is obtained by estimating the area under the curve between two temperature limits given by Equation 2.

(Equation 1)

Log in or to access full content. Learn more about your institution’s access to JoVE content here

Aplicação e Resumo

A major application area of DSC is the glass transition (Tg) in amorphous polymers, in which the material changes from a rigid glassy state to a viscous liquid state. Pharmaceutical research on nano-particles is also an emerging field, where the DSC has been used to quantify amorphous or crystalline phase in nano-solids. A review of DSC techniques on applications in biology and nano-science has been provided by Gill et al.3 Nanostructured lipid carriers (NLC) have potential applications in

Log in or to access full content. Learn more about your institution’s access to JoVE content here

Referências

  1. Robinson, J.W., Skelly Frame, E.M., Frame, GM. Undergraduate Instrumental Analysis. Marcel Decker, New York, NY. (2005).
  2. Liu, S., Li, C., Yu, J., Xiang, Q., Improved visible-light photocatalytic activity or porous carbon self-doped ZnO nanosheet-assembled flowers. CrystEngComm. 13, p 2533 (2011).
  3. Gill, P., Tohidu Moghadam, T., Ranjbar, B.  Differential Scanning Calorimetry Techniques: Applications in Biology and Nanoscience. Biomolecular Techniques. 21, 167-193 (2010).

Tags

Differential Scanning CalorimetryEnthalpyEnergy ChangesChemical ReactionsThermodynamicsConstant PressureExothermic ReactionsEndothermic ReactionsSafetyEfficiencyExperimentHeat FlowOxide DecompositionCarbonate Decomposition

Pular para...

0:00

Overview

1:23

Principles of Enthalpy

3:48

DSC Baseline Measurement

5:04

DSC Reference Measurement

6:22

Sample Measurement

7:10

Analysis of the DSC Data

8:42

Applications

10:56

Summary

Vídeos desta coleção:

article

Now Playing

Using Differential Scanning Calorimetry to Measure Changes in Enthalpy

General Chemistry

44.4K Visualizações

article

Common Lab Glassware and Uses

General Chemistry

653.4K Visualizações

article

Solutions and Concentrations

General Chemistry

273.1K Visualizações

article

Determining the Density of a Solid and Liquid

General Chemistry

554.7K Visualizações

article

Determining the Mass Percent Composition in an Aqueous Solution

General Chemistry

383.1K Visualizações

article

Determining the Empirical Formula

General Chemistry

180.0K Visualizações

article

Determining the Solubility Rules of Ionic Compounds

General Chemistry

141.1K Visualizações

article

Using a pH Meter

General Chemistry

344.3K Visualizações

article

Introduction to Titration

General Chemistry

423.4K Visualizações

article

Ideal Gas Law

General Chemistry

78.1K Visualizações

article

Spectrophotometric Determination of an Equilibrium Constant

General Chemistry

158.3K Visualizações

article

Le Châtelier's Principle

General Chemistry

264.0K Visualizações

article

Freezing-Point Depression to Determine an Unknown Compound

General Chemistry

160.4K Visualizações

article

Determining Rate Laws and the Order of Reaction

General Chemistry

195.7K Visualizações

article

Coordination Chemistry Complexes

General Chemistry

91.2K Visualizações

JoVE Logo

Privacidade

Termos de uso

Políticas

Pesquisa

Educação

SOBRE A JoVE

Copyright © 2025 MyJoVE Corporation. Todos os direitos reservados